Improved resistance of the coating on the electrode sheet to electrolyte
No abnormalities in appearance or adhesion after 7 days of immersion in electrolyte at 85°C
The use of a pre-treatment process prior to coating has significantly improved the adhesion of the coating to the electrode sheet